Article Notes
During lamination, EVA film passes through three stages. It softens under heat, flows around the cell string and interconnect ribs, and finally crosslinks into an insoluble network. Each stage has to happen in order: if the film gels before it has wetted the cells, air stays trapped at the cell edges.
Adhesion develops at both faces of the film. On the glass side the bond is optical and structural; on the cell side it locks the string in place and insulates the circuit. Holding the press at about 140–150 °C until gel content reaches at least 75% is the usual way to verify the cure has completed.